Comparision of Shear Bond Strength of Stainless Steel and Ceramic Brackets at 24 Hours after Etching Enamel with Different Proportions of Acidulated Phosphate Fluoride
ZC19-ZC21
Correspondence
Dr. Ramachandra Prabhakar,
Thai Moogambigai Dental College and Hospital,
Golden George Nagar, Chennai-600 107, India.
Phone : 9444171684, E-mail : dr.ramachandra.prabhakar@gmail.com
Aims and Objectives: To evaluate and compare the shear bond strength of stainless steel brackets and ceramic brackets at 24h after etching the enamel with acidulated phosphate fluoride gel (1.23% APF) at different proportions (40%,30%,20%) incorporated in conventional etchant (37% phosphoric acid).
Materials and Methods: Eighty premolars (maxillary and mandibular first and second premolars) extracted for orthodontic purpose has been selected for the study and samples were divided into 4 groups containing 10 teeth each. Comprised of teeth etched Group 1 with 40% of APF gel etchant is Group 2 teeth etched with 30% of APF gel in Group 3 teeth etched with 20% of APF gel etchant and Group 4 teeth were etched with conventional etchant (37% phosphoric acid).
Results: The experimental group of Acidulated Phosphate Fluoride (APF) at different proportion (40%, 30%, 20%) incorporated with etchant application for 40s on the enamel surface at 24h indicated that group 4 showed the higher bond strength of all other remaining groups and the groups 1, 2 and 3 showed satisfactory bond strength. The statistical evaluation also revealed that the bond strength of control group (37% phosphoric acid) was greater than those of experimental groups.
Conclusion: The present study results shows that the ceramic brackets have higher bond strength than stainless steel brackets (material wise).